Japan, May 13 -- JFE STEEL CORP has got intellectual property rights for 'AMMONIA STRESS CORROSION CRACKING ACCELERATION TEST METHOD.' Other related details are as follows:
Application Number: JP,2023-098072
Category (FI): G01N17/00,G01N33/2045,100
Stage: Grant (IP right granted following substantive examination.)
Filing Date: June 14, 2023
Publication Date: Dec. 26, 2024
The original document can be viewed at: https://www.j-platpat.inpit.go.jp/p0100